Preheat the steel carefully, heat to 1150 oC – 1200 oC maximum, hold until temperature is uniform throughout the section. Do not forge below 850 oC.Following forging operation the work piece should be cooled as slowly as possible.
Heat Treatment
Heat steels to 800 oC – 850 oC, hold until temperature is uniform throughout the section and cool in furnace.
Hardness
Anneal: ≤220HB Q+T: 28-34HRC HEAT TREAT MENT 55-62HRC
Application
1. Develop materials that are easy to process and good in polishing
With the production of optical disc, disk, prism and other precision parts, the demand for easy machining mirror steel increases. This kind of steel contains less non-metallic impurities, fine metallographic structure uniform, no fiber direction. It is the main development direction of plastic mold steel.
2. The corrosion resistant steel
In the process of long-term operation and maintenance of the mold, it is easy to rust and corrosion, and with the addition of various components in plastic molding, the mold is more prone to corrosion. Therefore, it is required to improve the corrosion resistance of the base material body, and some corrosion-resistant stainless steel has been developed.
3. Maraging alloy steel
This kind of steel has enough mechanical properties and outstanding process properties, especially high strength, toughness, wear resistance, low coefficient of thermal expansion, is a good steel for the manufacture of injection molding, but the price is expensive.
4. Cemented carbide
Mainly used in the production of high life requirements, the production of large batch of molds